    Both Zeron 100 and Zeron 100 FG meet the chemistry requirements of UNS S32760 and are made to a minimum PREn (pitting resistance equivalent) of 40 and are suitable for seawater service.
    All Zeron Tensile Classes viz; Zeron 100 FG, Zeron 100 FLT, Zeron 100 SA & Zeron 100 AFP meet the chemistry requirements of UNS S32760 and are made to a minimum PREn (pitting resistance equivalent) of 40 and are suitable for seawater service.

    Alloy Min Wrought (Cast), % Max Wrought (Cast), %
    Chromium (Cr) 24 26
    Nickel (Ni) 6.0 (6.5) 8.0 (8.5)
    Molybdenum (Mo) 3 4
    Tungsten (W) 0.5 1
    Copper (Cu) 0.5 1
    Nitrogen (N) 0.2 0.3
    Silicon (Si) 1
    Carbon (C) 0.03
    Manganese (Mn) 1
    Phosphorus (P) 0.03
    Sulfur (S) 0.01 (0.025)
    Iron (Fe) Balance  
    • * PREN = %Cr + 3.3 x %Mo + 16 x %N

    Cross-Grade Composition Comparison: S32760 vs S32750 vs Ferralium 255

    Procurement engineers comparing Zeron 100 to other super duplex alloys typically evaluate UNS S32750 (SAF 2507) and UNS S32550 (Ferralium 255). All three are "super duplex" per the PREN >= 40 definition but their compositions differ in W, Cu, and Mn additions.

    ElementUNS S32760 (Zeron 100 / F55)UNS S32750 (SAF 2507 / F53)UNS S32550 (Ferralium 255)
    Cr24.0-26.024.0-26.024.0-27.0
    Ni6.0-8.06.0-8.04.5-6.5
    Mo3.0-4.03.0-5.02.9-3.9
    N0.20-0.300.24-0.320.10-0.25
    Cu0.50-1.000.50 max1.50-2.50
    W0.50-1.00not addednot added
    Mn1.00 max1.20 max1.50 max
    PREN≥ 40≥ 40≥ 38

    Cross-reference: full Zeron 100 vs SAF 2507 comparison for mechanical and corrosion envelope detail.